ARP823F Minimizing Stress-Corrosion Cracking in Wrought High-Strength Aluminum Alloy Products
4/17/2019
- Content
- The purpose of this recommended practice is to provide the aerospace industry with recommendations concerning minimizing stress-corrosion cracking (SCC) in wrought high-strength aluminum alloy products.
- Citation
- SAE International Recommended Practice, Minimizing Stress-Corrosion Cracking in Wrought High-Strength Aluminum Alloy Products, SAE Standard ARP823F, Revised April 2019, Issued January 1964, https://doi.org/10.4271/ARP823F.