ARP823E Minimizing Stress-Corrosion Cracking in Wrought Heat-Treatable Aluminum Alloy Products
5/29/2013
- Content
- The purpose of this recommended practice is to provide the aerospace industry with recommendations concerning minimizing stress-corrosion cracking (SCC) in wrought high-strength aluminum alloy products.
- Pages
- 4
- Citation
- SAE International Recommended Practice, Minimizing Stress-Corrosion Cracking in Wrought Heat-Treatable Aluminum Alloy Products, SAE Standard ARP823E, Reaffirmed May 2013, Revised November 2007, Issued January 1964, https://doi.org/10.4271/ARP823E.