The data given in Tables 1–4 are typical values only and are not intended for design parameters. Mechanical properties of the special purpose alloys depend greatly upon processing variables and heat treatment. It is recommended that design data be obtained by actual testing or by consultation with the producers of the alloys.
Meta TagsDetails
DOI
https://doi.org/10.4271/J467B_196810
Pages
17
Citation
SAE International Information Report, SPECIAL PURPOSE ALLOYS ("SUPERALLOYS"), SAE Standard J467B_196810, Revised October 1968, Issued January 1956, https://doi.org/10.4271/J467B_196810.