AS5491A Calculation of Electron Vacancy Number in Superalloys

5/1/2001

Features
Issuing Committee
Scope
Content
This Aerospace Standard establishes a uniform procedure for calculation of electron vacancy numbers in superalloys. It is intended for use by suppliers of raw materials and parts, typically castings, for which control of electron vacancy number is required by the raw material specification.