Use of Cavitation Abrasive Surface Finishing to Improve the Fatigue Properties of Additive Manufactured Titanium Alloy Ti6Al4V
2021-01-0024
03/02/2021
- Event
- Content
- was 185 ± 9 MPa for the as-built DMLS specimen, 169 ± 14 MPa for the as-built EBM specimen, 425 ± 9 MPa for the DMLS specimen treated using CASF & cavitation peening, and 386 ± 9 MPa for the EBM specimen treated using CASF & cavitation peening.
- Citation
- Sanders, D., Soyama, H., and de Silva, C., "Use of Cavitation Abrasive Surface Finishing to Improve the Fatigue Properties of Additive Manufactured Titanium Alloy Ti6Al4V," SAE Technical Paper 2021-01-0024, 2021, .